CNCGLASS-Regular-Fogging-Defects-in-SGP-Glass

This article looks at regular fogging defects in SGP laminated glass, where every lite showed an internal veil in the same position and outline. The piece treats that repeating shape as an autoclave process signature and advises opening the load, correcting the hold, and cooling at no less than 3.3 degrees Celsius per minute before reworking the plates.

Published by Peter Lin CNC Glass Interlayer www.cncglass.com www.c-n-c.com Mail: cnc@cncglass.com benext77@hotmail.com

to order, please contact email: cnc@cncglass.com